Material Analysis
13 مشاهدة
CEF chemical resistance poor
ظاهرة المشكلة
After the CEF product is immersed in acid, alkali and solvent, the mechanical properties decrease by >30%
تحليل الأسباب
CEF has a high affinity for specific chemicals and is eroded and swollen; the CEF molecular chain is attacked and broken by chemicals
الحل
1) Select chemically resistant grades; 2) Slight crosslinking to reduce swelling; 3) Coating protection on the product surface; 4) Add chemical stabilizers
الخلاصة الأساسية
Poor chemical resistance is caused by the chemical affinity of CEF; selecting chemically resistant grades and coatings is the key
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!