Material Analysis 15 visualizaciones

CEF chemical resistance poor

Fenómeno del problema
After the CEF product is immersed in acid, alkali and solvent, the mechanical properties decrease by >30%
Análisis de la causa
CEF has a high affinity for specific chemicals and is eroded and swollen; the CEF molecular chain is attacked and broken by chemicals
Solución
1) Select chemically resistant grades; 2) Slight crosslinking to reduce swelling; 3) Coating protection on the product surface; 4) Add chemical stabilizers
Conclusión clave
Poor chemical resistance is caused by the chemical affinity of CEF; selecting chemically resistant grades and coatings is the key