Injection Molding
7 مشاهدة
Orange Peel Texture on CMC Surface
ظاهرة المشكلة
Orange-peel-like uneven texture on the surface of CMC products, rough to the touch
تحليل الأسباب
Mold temperature is low <30°C; the product surface cools and solidifies quickly, then the interior continues to shrink, causing surface unevenness; injection speed is too low
الحل
1)Increase mold temperature to 40-50°C to delay surface solidification; 2)Appropriately increase injection speed; 3)Increase holding pressure to reduce internal shrinkage
الخلاصة الأساسية
Orange peel is caused by rapid cooling and solidification; increasing mold temperature and holding pressure are the key
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا