Injection Molding 2 visualizaciones

Orange Peel Texture on CMC Surface

Fenómeno del problema
Orange-peel-like uneven texture on the surface of CMC products, rough to the touch
Análisis de la causa
Mold temperature is low <30°C; the product surface cools and solidifies quickly, then the interior continues to shrink, causing surface unevenness; injection speed is too low
Solución
1)Increase mold temperature to 40-50°C to delay surface solidification; 2)Appropriately increase injection speed; 3)Increase holding pressure to reduce internal shrinkage
Conclusión clave
Orange peel is caused by rapid cooling and solidification; increasing mold temperature and holding pressure are the key