Injection Molding
5 مشاهدة
MP obvious surface color difference
ظاهرة المشكلة
MP products have varying color depth at different locations, color difference ΔE>5
تحليل الأسباب
color masterbatch unevenly dispersed; pigment orientation during injection causing uneven color distribution; barrel temperature fluctuation causing color change
الحل
1) color masterbatch masterbatch method to ensure uniform dispersion; 2) reduce injection speed to reduce pigment orientation; 3) stabilize barrel temperature ±2°C
الخلاصة الأساسية
color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!