Injection Molding
7 visualizaciones
MP obvious surface color difference
Fenómeno del problema
MP products have varying color depth at different locations, color difference ΔE>5
Análisis de la causa
color masterbatch unevenly dispersed; pigment orientation during injection causing uneven color distribution; barrel temperature fluctuation causing color change
Solución
1) color masterbatch masterbatch method to ensure uniform dispersion; 2) reduce injection speed to reduce pigment orientation; 3) stabilize barrel temperature ±2°C
Conclusión clave
color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key