Extrusion & Post
12 مشاهدة
Analysis and Resolution of addition ratio of Smooth MB in PE blown film packaging film
ظاهرة المشكلة
When Smooth MB produces packaging film with PE blown film, abnormal performance related to addition ratio occurs.
تحليل الأسباب
The main cause is parameters deviating from the window in the aspect of addition ratio, leading to processing instability.
الحل
Comprehensively resolve the addition ratio problem from the perspective of formulation optimization.
الخلاصة الأساسية
The control of addition ratio of Smooth MB is the key link in ensuring processing quality.