Analysis and Resolution of addition ratio of Smooth MB in PE blown film packaging film
Problem Phenomenon
When Smooth MB produces packaging film with PE blown film, abnormal performance related to addition ratio occurs.
Cause Analysis
The main cause is parameters deviating from the window in the aspect of addition ratio, leading to processing instability.
Solution
Comprehensively resolve the addition ratio problem from the perspective of formulation optimization.
Key Takeaway
The control of addition ratio of Smooth MB is the key link in ensuring processing quality.