Extrusion & Post 6 مشاهدة

POE extrusion profile bending deformation

ظاهرة المشكلة
POE extruded profile shows continuous bending after cooling, bending amount >5mm/m
تحليل الأسباب
Uneven cooling of each face of the profile causes shrinkage differences; uneven die output flow velocity makes each wall thickness of the profile different; haul-off and extrusion centerline not aligned, producing lateral force
الحل
1) Optimize cooling system to ensure uniform cooling of each face; 2) Adjust the die so that flow velocity of each wall is uniform and wall thickness consistent; 3) Align haul-off with extrusion centerline; 4) Increase sizing sleeve length, cool after full sizing
الخلاصة الأساسية
Profile bending is caused by uneven cooling and uneven flow velocity; uniformization and alignment are the solution key
POE extrusionbending deformationuniform coolinguniform flow velocitysizing sleeve