Molding Process
2 مشاهدة
POE surface stress whitening
ظاهرة المشكلة
POE product stressed area surface stress whitening, affecting appearance and strength
تحليل الأسباب
POE under local stress, molecular orientation causes refractive index difference and whitening; product internal stress concentration areas
الحل
1) Reduce injection speed to reduce orientation stress; 2) Annealing treatment 80°C/2h to release stress; 3) Product design to avoid stress concentration sharp corners
الخلاصة الأساسية
Stress whitening is caused by orientation and internal stress; reducing orientation and annealing are key