High mold temperature requirement of PAR
ظاهرة المشكلة
The mold temperature needs 120-160°C, which conventional water temperature machines cannot meet.
تحليل الأسباب
PAR needs a high mold temperature (close to half of Tg, about 190°C) to reduce internal stress and ensure crystallization.
الحل
Use an oil temperature machine or electrically heated mold; the mold heating system design needs to consider high temperature.
الخلاصة الأساسية
PAR has special requirements for the mold heating system.