Ejector Whitening of PBT Injection-Molded Products
ظاهرة المشكلة
White patches or stress cracks appear at the ejector pin positions when PBT products are demolded.
تحليل الأسباب
The ejection force is too large or the ejector pin area is too small, and the local stress exceeds the limit; the draft angle is insufficient, increasing the demolding force; the cooling is insufficient and the strength is not enough.
الحل
Increase the ejector pin area or increase the number; increase the draft angle ≥2°; extend the cooling time.
الخلاصة الأساسية
PBT ejector whitening is the result of excessive local stress.