ظاهرة المشكلة
Streaks, uneven thickness or pinholes appear when coating functional coatings on PET film.
تحليل الأسباب
Film surface tension is uneven (locally insufficient dyne value); the coating liquid wets the film poorly; environmental cleanliness is insufficient.
الحل
Ensure uniform corona treatment, all areas ≥42mN/m; optimize the coating liquid formulation to improve wettability; operate in a clean environment.
الخلاصة الأساسية
PET film coating uniformity depends on surface treatment quality and coating process control.