Extrusion & Post
6 visualizações
Uneven coating on PET film
Fenómeno do problema
Streaks, uneven thickness or pinholes appear when coating functional coatings on PET film.
Análise das causas
Film surface tension is uneven (locally insufficient dyne value); the coating liquid wets the film poorly; environmental cleanliness is insufficient.
Solução
Ensure uniform corona treatment, all areas ≥42mN/m; optimize the coating liquid formulation to improve wettability; operate in a clean environment.
Conclusão principal
PET film coating uniformity depends on surface treatment quality and coating process control.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!