Blow Molding 9 مشاهدة

Increased brittleness of PA12 in extremely low temperature environments (below -40°C)

ظاهرة المشكلة
The brittleness of PA12 increases in extremely low temperature environments (below -40°C), affecting low-temperature applications
تحليل الأسباب
(1)The long carbon chain structure of PA12 restricts molecular chain movement at extremely low temperatures (2)Although PA12 is resistant to low temperature (-40°C), its performance declines at lower temperatures (3)The flexibility advantage of PA12 weakens in low-temperature environments (4)Adding plasticizers improves low-temperature performance but affects other properties (5)Comparison of low-temperature resistance grades of PA12 and PA11
الحل
(1)Select low-temperature-resistant PA12 modified varieties (2)Use PA12 with low-temperature toughening agents for use below -40°C (3)Evaluate the actual low-temperature requirements and select suitable materials (4)Compare the low-temperature performance with PA11 (5)Optimize the formulation to improve low-temperature toughness
الخلاصة الأساسية
PA12 low-temperature applications need to evaluate actual requirements
PA12low-temperature brittlenesslow-temperature resistancetoughening