Blow Molding 9 مشاهدة

Improper parison wall thickness, temperature, and length control affecting blow molded product quality

ظاهرة المشكلة
Improper parison wall thickness, temperature, and length control affects blow molded product quality
تحليل الأسباب
Insufficient parison wall thickness control accuracy Uneven parison temperature, severe sag Parison length control deviation Unstable parison extrusion speed Styrene-butadiene transparent resin (K resin) parison viscoelasticity affects wall thickness distribution
الحل
Use a wall thickness controller to precisely control parison wall thickness Stabilize parison extrusion temperature to reduce sag Precisely control parison length Stabilize parison extrusion speed Adjust parison parameters according to styrene-butadiene transparent resin (K resin) viscoelasticity
الخلاصة الأساسية
Parison needs precise control of wall thickness and temperature
parison controlwall thicknesstemperature'2079851475616104457