Extrusion & Post 6 مشاهدة

Pits, pinholes, or uneven coating on the surface of MABS products after electroplating

ظاهرة المشكلة
Pits, pinholes, or uneven coating appear on the surface of MABS products after electroplating
تحليل الأسباب
Improper MABS roughening process parameters Incomplete cleaning before electroplating, residual grease MABS rubber component affects roughening uniformity Insufficient activation treatment Improper electroplating solution composition or temperature
الحل
Optimize the MABS dedicated roughening process Thoroughly clean to remove grease Adjust roughening time considering the MABS rubber component Full activation treatment Adjust electroplating solution formulation and temperature
الخلاصة الأساسية
MABS electroplating needs dedicated roughening and activation processes
MABSelectroplatingrougheningcoating quality