Pits, pinholes, or uneven coating on the surface of MABS products after electroplating

Problembeschreibung
Pits, pinholes, or uneven coating appear on the surface of MABS products after electroplating
Ursachenanalyse
Improper MABS roughening process parameters Incomplete cleaning before electroplating, residual grease MABS rubber component affects roughening uniformity Insufficient activation treatment Improper electroplating solution composition or temperature
Lösung
Optimize the MABS dedicated roughening process Thoroughly clean to remove grease Adjust roughening time considering the MABS rubber component Full activation treatment Adjust electroplating solution formulation and temperature
Wichtigste Erkenntnis
MABS electroplating needs dedicated roughening and activation processes
MABSelectroplatingrougheningcoating quality