إجابات عملية على التحديات الشائعة في مواد البلاستيك

11636 سؤال
Q
MP '2079851475616104452 mold venting burning
Q
MP extrusion pelletizing connected pellets
A
connected pellets are caused by elastic recovery and low-temperature pelletizing; high-temperature water cutting and fast cutting are key
Extrusion & Post MP pelletizing connected pellets pelletizing water temperature cutter speed elastic recovery
Q
MP extrusion '2079851475616104457 severe parison sag
A
parison sag is caused by low melt strength; slight crosslinking and wall thickness control are key
Blow Molding MP '2079851475616104457 parison sag melt strength slight crosslinking wall thickness control
Q
poor interfacial bonding between MP and filler
Q
MP products yellowing after processing
A
Q
MP product dimensional change during long-term storage
A
dimensional change is caused by physical aging; annealing and slight crosslinking are measures to stabilize dimensions
Material Analysis MP dimensional stability physical aging annealing secondary crystallization slight crosslinking
Q
MP extrusion melt fracture
Q
MP '2079851475616104452 difficult demolding
Q
MP '2079851475616104452 thick-wall bubbles
A
thick-wall bubbles are caused by a combination of insufficient holding, moisture and poor venting
Material Drying MP injection bubble holding pressure thick-wall product mold venting
Q
Glass Fibre product elliptical deformation
A
elliptical deformation is caused by asymmetric demolding force; uniform ejection is key
Molds & Tooling Glass Fibre elliptical deformation symmetric ejection uniform cooling setting time