المشاكل والحلول

إجابات عملية على التحديات الشائعة في مواد البلاستيك

11636 سؤال
Q
Insufficient PVA toughness, brittle fracture
A
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is the key
Material Analysis PVAinsufficient toughnessmolecular weightcrosslinking controlcrystallization refinement
Q
Large fluctuation of PVA impact strength
A
Impact fluctuation is caused by unstable dispersed phase and crystallization; stable processing is the key
Molding Process PVAimpact fluctuationdispersed phase particle sizenucleating agentprocessing stability
Q
Poor PVA chemical resistance
A
Poor chemical resistance is caused by PVA chemical affinity; selecting chemical-resistant grade and coating are the key
Material Analysis PVAchemical resistancechemical attackslight crosslinkingsurface coating
Q
Large odor in PVA processing
A
Large odor is caused by PVA decomposition and volatilization; temperature control and ventilation are the key
Material Analysis PVAprocessing odorvolatilesventilation and exhausttemperature control
Q
PVA internal shrinkage voids
Q
Large PVA creep deformation
A
Large creep is caused by the elastomer nature; slight crosslinking and rigid filler are the key
Material Analysis PVAcreepslight crosslinkinghigh molecular weightrigid filler
Q
Poor PVA antistatic effect
A
Poor antistatic effect is caused by insufficient addition; increasing the antistatic agent is the key
Molding Process PVAantistaticantistatic agentsurface resistancemigration rate
Q
PVA processing temperature fluctuation
Q
Insufficient PVA tensile strength
A
Q
PVA screw slipping
A
Screw slipping is caused by premature melting; lowering the feed section temperature is the key
Extrusion & Post PVAscrew slippingfeed section temperaturepremature meltingflight deepening