Material Drying
3 Aufrufe
ASA Bubbles and Air Pockets
Problembeschreibung
【Problem Phenomenon】Bubbles inside ASA products, holes visible on sectioning, strength affected
Ursachenanalyse
Moisture vaporization, degradation gas generation and thick-wall shrinkage cavities are the three types of bubbles: moisture type distributed overall, degradation type accompanied by discoloration, shrinkage cavity type concentrated in thick-wall core; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience
Lösung
Locate the cause according to bubble distribution; moisture type strengthens drying, degradation type lowers temperature and shortens residence, shrinkage cavity type strengthens holding pressure; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Wichtigste Erkenntnis
ASA bubbles are classified by distribution, symptomatic treatment is effective; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
War das hilfreich?