Extrusion & Post 2 Aufrufe

HDPE pipe ovality out of tolerance

Problembeschreibung
The pipe cross-section is elliptical, affecting welding and laying.
Ursachenanalyse
Insufficient vacuum sizing, uneven cooling, or mismatch between haul-off speed and extrusion speed; the self-weight sag of large-diameter pipes also aggravates the ovality.
Lösung
①Adjust the vacuum degree of the vacuum tank; ②ensure uniform circumferential cooling of the pipe (uniform spraying/immersion); ③synchronize extrusion and haul-off speeds; ④calibrate the sizing sleeve dimensions.
Wichtigste Erkenntnis
Ovality = a synchronization problem of sizing + cooling + haul-off.
HDPE; pipe; ovality; vacuum sizing; haul-off