Injection Molding 8 Aufrufe

HDPE '2079851475616104452 warpage

Problembeschreibung
HDPE injection molded parts warp after ejection; common in drum lids and turnover crates.
Ursachenanalyse
HDPE has a high shrinkage rate (1.5%~3%) and strong crystallization directionality; uneven cooling and orientation cause differential shrinkage.
Lösung
①Balance the mold temperature; ②extend cooling; ③lower the holding pressure; ④optimize the gate position; ⑤homogenize the wall thickness.
Wichtigste Erkenntnis
HDPE '2079851475616104452 warpage = a cooling balance lesson for high-shrinkage materials.
HDPE; '2079851475616104452; warpage; shrinkage rate; cooling