Problembeschreibung
Thin flash appears at the parting line and ejector pins, often accompanied by clamping alarms.
Ursachenanalyse
Under high-pressure filling, the cavity pressure exceeds the clamping force; PC requires high injection pressure and is more likely to push the mold open; parting line wear or insufficient clamping tonnage is the direct cause.
Lösung
①Reduce injection/holding pressure; ②Calculate and increase the clamping force; ③Repair the parting line; ④Advance the holding pressure switchover point to avoid over-filling.
Wichtigste Erkenntnis
With PC's high-pressure process, the clamping margin must be left sufficient.