Extrusion & Post
2 Aufrufe
PC Printing and Painting
Problembeschreibung
[Problem Phenomenon] PC products require printing and painting decoration
Ursachenanalyse
PC surfaces can be printed and painted with relatively good adhesion; it is ready after cleaning to remove mold release agent; IMD/IML processes are mature; when troubleshooting on site, verify each item according to this mechanism one by one, and avoid blindly adjusting the machine based on experience alone
Lösung
Clean before printing and painting; select matching processes for IMD; adhesion testing; after adjustment, take samples continuously to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Wichtigste Erkenntnis
PC printing and painting have good adhesion; IMD is mature; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
War das hilfreich?
0 Personen fanden dies hilfreich