Molds & Tooling 2 Aufrufe

PEI Internal Stress Cracking

Problembeschreibung
PEI products generate internal stress during cooling, leading to deformation or cracking; cracks mostly originate from sharp corners and assembly stress points.
Ursachenanalyse
PEI's glass transition temperature is as high as 217℃, and fast cooling freezes molecular chains with large stress; excessive cooling speed or unreasonable mold design accumulates internal stress; unreleased stress triggers cracking during use.
Lösung
①Use a high-temperature mold with mold temperature of 140~180℃ to reduce internal stress; ②sufficient cooling time but avoid overcooling; ③eliminate sharp corners in the structure with rounded transitions; ④anneal when necessary.
Wichtigste Erkenntnis
PEI internal stress management revolves around high mold temperature; the 217℃ Tg determines the process temperature level; structural rounded corners are the design bottom line.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PEI;internal stress;cracking;mold temperature;Tg;annealing