Molds & Tooling 2 Aufrufe

PMMA Short Shot

Problembeschreibung
Thin-wall long-flow material shortage.
Ursachenanalyse
PMMA melt viscosity is high and flow is slow; insufficient pressure and speed, low mold temperature.
Lösung
①Increase the injection pressure (60~120MPa); ②Raise melt temperature and mold temperature; ③Large gate; ④Optimize the runner.
Wichtigste Erkenntnis
PMMA short shot = the pressure account of high viscosity.
PMMA; short shot; viscosity; injection pressure; mold temperature