Molds & Tooling 1 views

PMMA Short Shot

Problem Phenomenon
Thin-wall long-flow material shortage.
Cause Analysis
PMMA melt viscosity is high and flow is slow; insufficient pressure and speed, low mold temperature.
Solution
①Increase the injection pressure (60~120MPa); ②Raise melt temperature and mold temperature; ③Large gate; ④Optimize the runner.
Key Takeaway
PMMA short shot = the pressure account of high viscosity.
PMMA; short shot; viscosity; injection pressure; mold temperature