Molds & Tooling 4 Aufrufe

PPO Melt Fracture

Problembeschreibung
During high-speed filling of PPO, melt fracture patterns appear on the product surface; reducing speed leads to insufficient filling, and the contradiction is prominent in thin-walled parts.
Ursachenanalyse
The high-viscosity PPO melt has a low critical shear rate, and high-speed filling easily triggers melt fracture; small gates concentrate shear; low temperature increases viscosity and aggravates the fracture tendency.
Lösung
①Multi-stage injection with reduced speed in the gate area and increased speed in the filling area; ②enlarge the gate to reduce shear rate; ③increase melt temperature to reduce viscosity; ④switch to a high-flow grade if necessary.
Wichtigste Erkenntnis
The contradiction between PPO melt fracture and insufficient filling is resolved by multi-stage injection; gate size is a structural solution; high-flow grades are a material-level way out.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PPO; melt fracture; shear; multi-stage injection; gate; thin wall