Extrusion & Post 9 Aufrufe

Severe EEA extruder screw wear

Problembeschreibung
After 200h of EEA extrusion, screw and barrel wear reaches 0.5mm
Ursachenanalyse
Filler causes large wear on the screw; insufficient screw material hardness, not nitrided; processing temperature too high causing EEA to adhere to the screw and aggravate wear
Lösung
1) Use nitrided screw or bimetallic screw SK-2 alloy; 2) Reduce processing temperature to reduce adhesive wear; 3) Treat filler with coupling agent to reduce friction; 4) Regularly check wear, replace in time when >0.3mm
Wichtigste Erkenntnis
Screw wear is caused by filler friction and adhesion; wear-resistant screw and temperature control are the key
EEA extrusionscrew wearnitrided screwfiller frictionbimetallic screw