Dense EMA surface pits
Problembeschreibung
0.1-0.3mm dense pits on EMA product surface affect appearance and coating adhesion
Ursachenanalyse
Raw material contains impurity particles >0.05%; mold cavity surface damage or corrosion pits
Lösung
1) Replace with pure raw material with impurities <0.01%; 2) Repair and polish mold cavity to Ra<0.2μm; 3) Filter raw material to remove particles
Wichtigste Erkenntnis
Pits are caused by raw material impurities and mold damage; pure raw material and mold maintenance are key