Dense EMA surface pits
Fenómeno del problema
0.1-0.3mm dense pits on EMA product surface affect appearance and coating adhesion
Análisis de la causa
Raw material contains impurity particles >0.05%; mold cavity surface damage or corrosion pits
Solución
1) Replace with pure raw material with impurities <0.01%; 2) Repair and polish mold cavity to Ra<0.2μm; 3) Filter raw material to remove particles
Conclusión clave
Pits are caused by raw material impurities and mold damage; pure raw material and mold maintenance are key
¿Le ha resultado útil?
0 personas encontraron esto útil