Extrusion & Post 9 Aufrufe

EMA vacuum vent overflow

Problembeschreibung
EMA extrusion vacuum section overflows, clogging the vent hole
Ursachenanalyse
EMA melt viscosity low, overflowing at the vacuum section; vacuum section temperature too high making viscosity even lower and worsening overflow; improper vent hole design
Lösung
1) Lower vacuum section temperature by 5-10°C to increase viscosity; 2) Add baffle above the vent hole to prevent overflow; 3) Increase screw speed to accelerate conveying and reduce residence time
Wichtigste Erkenntnis
Overflow is caused by low melt viscosity; temperature reduction and baffle addition are key
EMA vacuum section overflow melt viscosity temperature reduction vent baffle