Extrusion & Post
9 Aufrufe
EVA extruded film has gel particles
Problembeschreibung
Transparent gel particles of 0.1-0.5mm appear on the surface of EVA extruded film
Ursachenanalyse
High molecular weight components in EVA are not fully melted during extrusion, forming local highly crystalline regions; extrusion temperature too low or insufficient mixing
Lösung
1) Increase extrusion temperature by 5-10°C to ensure full melting; 2) Increase the length of the screw mixing section; 3) Inspect raw material to ensure consistent grade; 4) Replace with a finer 120-mesh screen to intercept unmelted particles
Wichtigste Erkenntnis
Gel particles are caused by insufficient melting; increasing temperature and mixing are key
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!