Processing Machinery 3 Aufrufe

EVA internal unmelted particles

Problembeschreibung
Unmelted transparent or translucent particles appear inside EVA products
Ursachenanalyse
Insufficient screw plasticizing capacity with low temperature; feeding amount too large exceeding the plasticizing capacity; EVA melting temperature too high
Lösung
1) Increase processing temperature to ensure full melting; 2) Reduce feeding amount to match plasticizing capacity; 3) Increase the screw mixing section
Wichtigste Erkenntnis
Unmelted particles are caused by insufficient plasticization; increasing temperature and reducing feeding are key
EVA unmelted particles plasticizing capacity processing temperature screw mixing