EVA internal unmelted particles

Fenómeno do problema
Unmelted transparent or translucent particles appear inside EVA products
Análise das causas
Insufficient screw plasticizing capacity with low temperature; feeding amount too large exceeding the plasticizing capacity; EVA melting temperature too high
Solução
1) Increase processing temperature to ensure full melting; 2) Reduce feeding amount to match plasticizing capacity; 3) Increase the screw mixing section
Conclusão principal
Unmelted particles are caused by insufficient plasticization; increasing temperature and reducing feeding are key