EVA internal unmelted particles
Fenómeno del problema
Unmelted transparent or translucent particles appear inside EVA products
Análisis de la causa
Insufficient screw plasticizing capacity with low temperature; feeding amount too large exceeding the plasticizing capacity; EVA melting temperature too high
Solución
1) Increase processing temperature to ensure full melting; 2) Reduce feeding amount to match plasticizing capacity; 3) Increase the screw mixing section
Conclusión clave
Unmelted particles are caused by insufficient plasticization; increasing temperature and reducing feeding are key