EVOH extruded film thickness uniformity is poor

Problembeschreibung
EVOH extruded film transverse thickness deviation ±15%, exceeding the ±5% industry standard
Ursachenanalyse
Unreasonable die flow channel design causing uneven melt flow in the wide die; EVOH melt elasticity large with uneven extrusion swell; uneven air ring cooling
Lösung
1) Adopt coat-hanger die design to ensure uniform transverse flow; 2) Fine-tune die gap ±0.02mm; 3) Optimize air ring air volume and angle for uniform cooling; 4) Add a small amount of low-elasticity resin to reduce swell differences
Wichtigste Erkenntnis
Film thickness uniformity requires coordinated optimization from die design, gap adjustment, and cooling
EVOH film thickness uniformity die design extrusion swell air ring cooling