Extrusion & Post 13 visualizações

EVOH extruded film thickness uniformity is poor

Fenómeno do problema
EVOH extruded film transverse thickness deviation ±15%, exceeding the ±5% industry standard
Análise das causas
Unreasonable die flow channel design causing uneven melt flow in the wide die; EVOH melt elasticity large with uneven extrusion swell; uneven air ring cooling
Solução
1) Adopt coat-hanger die design to ensure uniform transverse flow; 2) Fine-tune die gap ±0.02mm; 3) Optimize air ring air volume and angle for uniform cooling; 4) Add a small amount of low-elasticity resin to reduce swell differences
Conclusão principal
Film thickness uniformity requires coordinated optimization from die design, gap adjustment, and cooling
EVOH film thickness uniformity die design extrusion swell air ring cooling