Processing Machinery
3 Aufrufe
Insufficient EVOH Mixing
Problembeschreibung
After blending EVOH with fillers/additives, dispersion is uneven with local agglomeration
Ursachenanalyse
Screw mixing section length insufficient; kneading block quantity not enough; feeding method improper, additives not fully contacting EVOH
Lösung
1) Increase screw mixing section length to 3-4D; 2) Increase kneading block quantity; 3) Add additives after the side feeding port to increase mixing time
Wichtigste Erkenntnis
Insufficient mixing is caused by improper screw design; increasing mixing section is key
War das hilfreich?
0 Personen fanden dies hilfreich