Processing Machinery 8 visualizaciones

Insufficient EVOH Mixing

Fenómeno del problema
After blending EVOH with fillers/additives, dispersion is uneven with local agglomeration
Análisis de la causa
Screw mixing section length insufficient; kneading block quantity not enough; feeding method improper, additives not fully contacting EVOH
Solución
1) Increase screw mixing section length to 3-4D; 2) Increase kneading block quantity; 3) Add additives after the side feeding port to increase mixing time
Conclusión clave
Insufficient mixing is caused by improper screw design; increasing mixing section is key
EVOHinsufficient mixingscrew mixing sectionkneading blockside feeding