Insufficient EVOH Mixing
Fenómeno do problema
After blending EVOH with fillers/additives, dispersion is uneven with local agglomeration
Análise das causas
Screw mixing section length insufficient; kneading block quantity not enough; feeding method improper, additives not fully contacting EVOH
Solução
1) Increase screw mixing section length to 3-4D; 2) Increase kneading block quantity; 3) Add additives after the side feeding port to increase mixing time
Conclusão principal
Insufficient mixing is caused by improper screw design; increasing mixing section is key