Molds & Tooling 3 Aufrufe

Insufficient roundness of PU

Problembeschreibung
Roundness deviation of PU round products >0.3mm
Ursachenanalyse
Uneven cooling causing different shrinkage in each direction; gate position causing local over-filling; asymmetric demolding force
Lösung
1) Annular uniform cooling to ensure consistent shrinkage in all directions; 2) Symmetrical arrangement of gate positions; 3) Uniform ejection to avoid deformation
Wichtigste Erkenntnis
Insufficient roundness is caused by uneven cooling; annular cooling is key
PU insufficient roundness uniform cooling gate symmetry demolding force