Back to Problem & Solution
Molds & Tooling 2 views

Insufficient roundness of PU

Problem Phenomenon
Roundness deviation of PU round products >0.3mm
Cause Analysis
Uneven cooling causing different shrinkage in each direction; gate position causing local over-filling; asymmetric demolding force
Solution
1) Annular uniform cooling to ensure consistent shrinkage in all directions; 2) Symmetrical arrangement of gate positions; 3) Uniform ejection to avoid deformation
Key Takeaway
Insufficient roundness is caused by uneven cooling; annular cooling is key
PU insufficient roundness uniform cooling gate symmetry demolding force