Material Analysis
10 Aufrufe
Poor resilience of PU flexible foam
Problembeschreibung
PU flexible foam resilience <40%, below 60%
Ursachenanalyse
Isocyanate index too high >1.1; foam density too high; improper catalyst formulation
Lösung
1) Lower isocyanate index to 0.95-1.0; 2) Increase blowing agent to reduce density; 3) Adjust catalyst formulation
Wichtigste Erkenntnis
PU flexible foam resilience is determined by isocyanate index and catalyst formulation