Poor resilience of PU flexible foam
문제 현상
PU flexible foam resilience <40%, below 60%
원인 분석
Isocyanate index too high >1.1; foam density too high; improper catalyst formulation
해결 방법
1) Lower isocyanate index to 0.95-1.0; 2) Increase blowing agent to reduce density; 3) Adjust catalyst formulation
핵심 요약