Extrusion & Post 9 Aufrufe

Longitudinal stripes on PVA extruded film

Problembeschreibung
Continuous stripes 1-3mm wide along the extrusion direction on the surface of PVA extruded film
Ursachenanalyse
Local damage or uneven gap of die lips; melt residence zone in the die producing unstable flow; pressure fluctuation at the screw front end
Lösung
1) Check die lip flatness and gap uniformity ±0.01mm; 2) Clean the die interior to remove carbonized matter in the residence zone; 3) Install gear pump on the extruder to stabilize melt pressure; 4) Polish die lips to Ra<0.1μm
Wichtigste Erkenntnis
Longitudinal stripes are caused by die defects and pressure fluctuation; die maintenance and pressure stability are key
PVA film longitudinal stripes die gap melt pressure lip flatness