Molding Process 6 Aufrufe

PVA water-soluble film dissolution rate mismatch

Problembeschreibung
PVA water-soluble film dissolution time deviation at target temperature >30%
Ursachenanalyse
PVA alcoholysis degree does not match the application temperature requirement; large film thickness deviation
Lösung
1) Select PVA alcoholysis degree matching the target dissolution temperature; 2) Film thickness precise ±5%; 3) Adjust formulation liquid to adjust dissolution rate
Wichtigste Erkenntnis
PVA water-soluble film dissolution rate is determined by alcoholysis degree and thickness
PVA water-soluble filmdissolution ratealcoholysis degreefilm thicknessformulation adjustment