PVA water-soluble film dissolution rate mismatch
문제 현상
PVA water-soluble film dissolution time deviation at target temperature >30%
원인 분석
PVA alcoholysis degree does not match the application temperature requirement; large film thickness deviation
해결 방법
1) Select PVA alcoholysis degree matching the target dissolution temperature; 2) Film thickness precise ±5%; 3) Adjust formulation liquid to adjust dissolution rate
핵심 요약
PVA water-soluble film dissolution rate is determined by alcoholysis degree and thickness