Molding Process 8 görüntüleme

PVA water-soluble film dissolution rate mismatch

Sorun Belirtisi
PVA water-soluble film dissolution time deviation at target temperature >30%
Neden Analizi
PVA alcoholysis degree does not match the application temperature requirement; large film thickness deviation
Çözüm
1) Select PVA alcoholysis degree matching the target dissolution temperature; 2) Film thickness precise ±5%; 3) Adjust formulation liquid to adjust dissolution rate
Temel Çıkarım
PVA water-soluble film dissolution rate is determined by alcoholysis degree and thickness
PVA water-soluble filmdissolution ratealcoholysis degreefilm thicknessformulation adjustment